20MnCrS5 is an alloy material with excellent performance. It is suitable for manufacturing mechanical parts with requirements on strength, hardness and wear resistance. It is one of the important materials in the field of mechanical manufacturing, such as automobile manufacturing, mechanical equipment manufacturing, etc. Due to its excellent mechanical properties and processing properties, it is widely used in the manufacture of various important parts, such as gears, bearings, transmission shafts, etc.
Availability:
Quantity:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
sharethis sharing button

CHEMICAL COMPOSITION

C: 0.17-0.22

Si: ≤ 0.4

Mn: 1.1-1.4

P: ≤ 0.025

S: 0.02-0.04

Cr: 1.0-1.3



MECHANICAL PROPERTIES

Tensile strength: ≥ 850MPa

Yield strength: ≥ 700MPa

Elongation: ≥ 12%

Hardness: ≤ 217HB

Toughness: Good



HEAT TREATMENT

Normalizing,°C: 840-870

Annealing,°C: 650-700

Carburizing,°C: 880-980

Core Hardening,°C:  860-900

Case Hardening,°C: 780-820

Tempering,°C:  150-200


The Management and Staff at Union Steel, have a firm belief that by identifying the customers’ needs, we can achieve the best results for all. Union Steel warmly welcomes friends around the world to cooperate with us.

Quick Links

Contact Us

Tel: +86-24-81267300
Phone: +86-18904079192
Add: No. 237, Shenbei West Road, Yuhong District, Shenyang City, Liaoning Province

Product Category

Keep In Touch
Contact
Copyright ©  2024 Union Steel. All rights reserved.  SitemapPrivacy Policy  辽ICP备2024037155号-1