Availability: | |
---|---|
Quantity: | |
CHEMICAL COMPOSITION
C:≤0.22
Si:≤0.55
Mn:≤1.60
P:≤0.035
S:≤0.035
C.E.:≤0.047
MECHANICAL PROPERTIES
Thickness (mm): 3<thk<100
Yield Strength Rehmin (N / mm²): 355-550
Tensile Strength Rmmin (N / mm²): 490-630
Elongation A5 min(%): max 22
Impact Values Charpy-V-Notch Longitudinal Average from 3 Speimens Thk.>10 < 150mm.: 27 Joules at -20 C
HEAT TREATMENT
S355J2+N steel plate is delivered in normalized state by default. Heat treatment can include annealing, normalizing and tempering. The lower limit of tempering temperature is 675℃. S355J2+N steel plate can also be delivered in hot-rolled, controlled-rolled and other states. These states affect the microstructure and performance of the material.
CHEMICAL COMPOSITION
C:≤0.22
Si:≤0.55
Mn:≤1.60
P:≤0.035
S:≤0.035
C.E.:≤0.047
MECHANICAL PROPERTIES
Thickness (mm): 3<thk<100
Yield Strength Rehmin (N / mm²): 355-550
Tensile Strength Rmmin (N / mm²): 490-630
Elongation A5 min(%): max 22
Impact Values Charpy-V-Notch Longitudinal Average from 3 Speimens Thk.>10 < 150mm.: 27 Joules at -20 C
HEAT TREATMENT
S355J2+N steel plate is delivered in normalized state by default. Heat treatment can include annealing, normalizing and tempering. The lower limit of tempering temperature is 675℃. S355J2+N steel plate can also be delivered in hot-rolled, controlled-rolled and other states. These states affect the microstructure and performance of the material.