SAE4340 is a high-strength, low-alloy steel known for its outstanding toughness, strength and fatigue resistance, and is particularly suitable for applications such as aerospace, oil and gas, and the automotive industry. This material has excellent mechanical properties and wear resistance, and is often used to manufacture high-strength, high-wear-resistant parts, such as crankshafts for aircraft engines and gears for automotive transmissions. The development trend of SAE4340 steel focuses on improving material properties and production process improvements, while paying attention to environmental protection and sustainable development. This alloy steel plays an important role in the fields of aviation, automobiles, and energy due to its excellent performance and wide application prospects.
Availability:
Quantity:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
sharethis sharing button

CHEMICAL COMPOSITION

C: 0.38-0.43

Si: 0.15-0.35

Mn: 0.60-0.80

Cr: 0.7-0.9

Mo: 0.15-0.25

Ni: 1.65-2.0

P: ≤0.035

S: ≤0.04



MECHANICAL PROPERTIES

Yield strengths: 740-1860MPa

Tensile strengths: 860-1980MPa

Elongations: 11-23%



PHYSICAL PROPERTIES

Density, g/cm3: 7.87

Melting point,℃: 1408

Specific heat capacity,(0~100℃),J/(kg.k): 582(200℃)

Linear expansion coefficient,10^-6/k: 0~100℃/12.8

Poisson's ratio: 0.295

Elastic Modulus,Mpa: 213000

Shear modulus,Mpa: 82300

Resistivity,10^-8 Ω.m: 36.2(150℃)

Thermal conductivity,W/(m.K): 36.01(150℃)



HEAT TREATMENT

Complete annealing (recrystallization annealing):830-850°C

Isothermal annealing:650°C,keep temperature for 8 hours

Soft annealing: 670-700°C

Stress relief annealing:600-650°C

Ac1: 732℃

Ac3: 774℃

Ar1: 680℃


The Management and Staff at Union Steel, have a firm belief that by identifying the customers’ needs, we can achieve the best results for all. Union Steel warmly welcomes friends around the world to cooperate with us.

Quick Links

Contact Us

Tel: +86-24-81267300
Phone: +86-18904079192
Add: No. 237, Shenbei West Road, Yuhong District, Shenyang City, Liaoning Province

Product Category

Keep In Touch
Contact
Copyright ©  2024 Union Steel. All rights reserved.  SitemapPrivacy Policy  辽ICP备2024037155号-1