KOMPOSISYON NG KEMIKAL
C: 0.18-0.23
Si: 0.15-0.35
Mn: 0.5-0.9
P: ≤0.02
S: ≤0.02
Ni: ≤0.3
Cr: 0.85-1.25
Mo: 0.15-0.25
Cu: ≤0.2
Al: ≥0.015
MECHANICAL PROPERTIES
Lakas ng makunat (kgf/mm²): ≥95
Pagpahaba (%): ≥14
Rate ng pagbabawas ng cross section (%): ≥40
Halaga ng epekto (J/cm2): ≥6
Katigasan (Hb): 352-362
PISIKAL NA KATANGIAN
Modulus ng elasticity [103 x N/mm2]: 210
Densidad [g/cm3]: 7.85
Thermal conductivity [W/mK]: 20.0
Forging ng ASTM Grade 4118 Steel
Mainit na temperatura ng pagbuo: 1100-850oC.
PAGGAgamot sa init
Pagsusupil: 850 ℃ Paglamig ng Furnace
Normalization: 850~900 ℃ Paglamig ng Hangin
Pagpapatigas: 850-900 ℃ 1st Oil Cooling, 800-850 ℃ 2rd Oil Cooling