CHEMICAL COMPOSITION
C: 0.26
Si: 0.40
Mn: 1.03
P: 0.04
S: 0.05
Cu: 0.20
Fe: 98
MECHANICAL PROPERTIES
Tensile Strength, Ultimate: 400-550MPa; 58000-79800psi
Tensile Strength, Yield: 250MPa; 36300psi
Elongation at Break (in 200 mm): 20.0 %
Elongation at Break (in 50 mm): 23.0 %
Modulus of Elasticity: 200GPa; 29000ksi
Bulk Modulus (typical for steel): 140GPa; 20300ksi
Poissons Ratio: 0.260
Shear Modulus: 79.3GPa; 11500ksi
PHYSICAL PROPERTIES
Density: 7.85 g/cm3; 0.284 lb/in3
FORGING
According to the forging temperature, it can be divided into hot forging, warm forging and cold forging. Hot forging is usually carried out above 800℃, while warm forging or semi-hot forging is carried out between 300 and 800℃, and cold forging is carried out at room temperature. A36 steel is suitable for processing at different forging temperatures due to its good machinability.