CHEMICAL COMPOSITION
C: 0.38-0.43
Si: 0.15-0.35
Mn: 0.60-0.80
Cr: 0.7-0.9
Mo: 0.15-0.25
Ni: 1.65-2.0
P: ≤0.035
S: ≤0.04
MECHANICAL PROPERTIES
Yield strengths: 740-1860MPa
Tensile strengths: 860-1980MPa
Elongations: 11-23%
PHYSICAL PROPERTIES
Density, g/cm3: 7.87
Melting point,℃: 1408
Specific heat capacity,(0~100℃),J/(kg.k): 582(200℃)
Linear expansion coefficient,10^-6/k: 0~100℃/12.8
Poisson's ratio: 0.295
Elastic Modulus,Mpa: 213000
Shear modulus,Mpa: 82300
Resistivity,10^-8 Ω.m: 36.2(150℃)
Thermal conductivity,W/(m.K): 36.01(150℃)
HEAT TREATMENT
Complete annealing (recrystallization annealing):830-850°C
Isothermal annealing:650°C,keep temperature for 8 hours
Soft annealing: 670-700°C
Stress relief annealing:600-650°C
Ac1: 732℃
Ac3: 774℃
Ar1: 680℃